MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
SABIC ULTEM™ Resin ATX200 Polyetherimide (PEI) (Asia)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: High flow Polyetherimide blend. ECO Conforming, UL94 V0 Listing.

Features: High Stiffness,Hydrolytic Stability,Chemical Resistance,Low Smoke and Toxicity,Good Mechanicals in Broad Temperature Range,Low Creep Sensitivity,Low Shrinkage,Good metal adhesion,Amorphous,High Strength,High Heat Resistance,Good dimensional stability,Flame Retardant,High Impact Resistance

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.26 g/ccASTM D792
Moisture Absorption 0.0200 %Injection Molding
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 24 g/10 min
@Load 6.60 kg,
Temperature 337 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 96.0 MPa5 mm/min; ASTM D638
Elongation at Break 70 %5 mm/min; ASTM D638
Flexural Strength 144 MPayld, 2.6 mm/min, 100 mm span; ASTM D790
Flexural Modulus 3170 MPa2.6 mm/min, 100 mm span; ASTM D790
Izod Impact Notched 53.0 JASTM D256
 2136 J
@Thickness 3.20 mm
reverse notched; ASTM D256
Izod Impact, Unnotched 2082 J/mASTM D4812
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 100 - 175 VUL 746A
Hot Wire Ignition, HWI >= 120 sec
@Thickness >=0.750 mm
UL 746A
High Amp Arc Ignition, HAI 0.00 - 15 arcs
@Thickness >=0.750 mm
UL 746A
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 190 °C
@Thickness 6.40 mm
unannealed; ASTM D648
UL RTI, Electrical 115 °CUL 746B
UL RTI, Mechanical with Impact 115 °CUL 746B
UL RTI, Mechanical without Impact 115 °CUL 746B
Flammability, UL94 V-2
@Thickness >=0.750 mm
UL 94
 V-0
@Thickness >=1.50 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 350 - 370 °C
Zone 2 345 - 365 °C
Zone 3 350 - 370 °C
Melt Temperature 350 - 370 °CInjection Molding
Mold Temperature 135 - 165 °C
Drying Temperature 135 °CInjection Molding
Dry Time 4.00 - 6.00 hourInjection Molding
 10.0 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa
Shot Size 40 - 60 %
Vent Depth 0.00250 - 0.00760 cm
Screw Speed 40 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82647 / 290594

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.