MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
SABIC VALOX™ SHF4330 PBT (Europe)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: 15% GF reinforced PBT/ASA, High Flow version

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.39 g/ccASTM D792
Density 1.39 g/ccISO 1183
Filler Content 15 %ASTM D229
Viscosity 90 cP
@Shear Rate 1500 1/s,
Temperature 260 °C
melt; ISO 11443
Linear Mold Shrinkage, Flow 0.0020 - 0.0060 cm/cmSABIC method
Melt Flow 40 g/10 min
@Load 5.00 kg,
Temperature 250 °C
cm³/10 min; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 120ISO 2039-2
Ball Indentation Hardness 160 MPaISO 2039-1
Tensile Strength at Break 85.0 MPa5 mm/min; ASTM D638
 85.0 MPa5 mm/min; ISO 527
Tensile Strength, Yield 85.0 MPa5 mm/min; ASTM D638
 85.0 MPa5 mm/min; ISO 527
Elongation at Break 3.0 %5 mm/min; ISO 527
 3.0 %5 mm/min; ASTM D638
Elongation at Yield 3.0 %5 mm/min; ASTM D638
 3.0 %5 mm/min; ISO 527
Tensile Modulus 5300 MPa5 mm/min; ASTM D638
 5400 MPa1mm/min; ISO 527
Flexural Strength 120 MPa2 mm/min; break; ISO 178
Flexural Yield Strength 120 MPa2 mm/min; ISO 178
Flexural Modulus 4800 MPa2 mm/min; ISO 178
Flexural Strain at Break 3.0 %2 mm/min; ISO 178
Izod Impact, Notched (ISO) 4.00 kJ/m²80*10*4; ISO 180/1A
 4.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 28.0 kJ/m²80*10*4; ISO 180/1U
 20.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1U
Charpy Impact Unnotched 30.0 kJ/m²ISO 179/2C
 20.0 kJ/m²
@Temperature -30.0 °C
ISO 179/2C
Charpy Impact, Notched 4.00 kJ/m²ISO 179/2C
 4.00 kJ/m²
@Temperature -30.0 °C
ISO 179/2C
 
Thermal PropertiesOriginal ValueComments
Hot Ball Pressure Test 125 °CIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 204 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 152 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
Vicat Softening Point 157 °CRate B/50; ISO 306
 159 °CRate B/120; ISO 306
 215 °CRate A/50; ISO 306
 
Processing PropertiesOriginal ValueComments
Processing Temperature 40.0 - 60.0 °CHopper Temperature
Nozzle Temperature 240 - 260 °CInjection Molding
Zone 1 230 - 245 °C
Zone 2 240 - 255 °C
Zone 3 245 - 265 °C
Melt Temperature 250 - 270 °C
Mold Temperature 40.0 - 100 °C
Drying Temperature 110 - 120 °CInjection Molding
Dry Time 2.00 - 4.00 hourInjection Molding
Moisture Content 0.020 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10289 / 243756

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.