Product description: Sodium diisooctylsulfosuccinate Application: REWOPOL® SB DO 75 is used in textile industry as rapid wetting agent and antistat in spin finishes. Properties / Benefits: REWOPOL® SB DO 75 is an anionic surfactant, miscible with non-ionic, amphoteric and other anionic products. REWOPOL® SB DO 75 has good oil solubility and antistatic properties. It is a highly effective emulsifier with very good wetting properties. Information provided by Evonik |