Overview: CALIBRE™ 300V Polycarbonate resins offer exceptional impact resistance, heat distortion resistance, optical clarity and meets UL94 V-2 rating. CALIBRE 300V series products are available in 3 additive packages: CALIBRE 301V: Mold release. CALIBRE 302V: UV stabilizer. CALIBRE 303V: Mold release and UV stabilizer. Govt. and Industry Standards: - CSA (Canadian Standards Association)
- Underwriters Laboratory Inc. (UL)
Applications:- Electronic components
- Lighting
- Storage Media Housings
Information provided by Styron |