Applications include high-speed screw machine products where superior machining characteristics of this steel can be fully utilized. |
UNS G12134, ASTM A29, FED QQ-S-633(C12l13), MIL SPEC MIL-S-18411, SAE J403, JIS SUM 24 L, SS14 1914 (Sweden), SAE J412, DIN 1.0718, UNI 9SMnPb23, JIS SUM 22 L, JIS SUM 23 L |