MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Oxygen-free high conductivity Copper, Soft, UNS C10200
Categories: Metal; Nonferrous Metal; Copper Alloy; Wrought Copper

Material Notes: Applications: busbars, bus conductors, waveguides, hollow conductors, lead-in wires and anodes for vacuum tubes, vacuum seals, transistor components, glass to metal seals, coaxial cables, klystrons, microwave tubes, and rectifiers.

Processing: Excellent hot and cold workability; good forgeability. Fabricated by bending, coining, coppersmithing, drawing and upsetting, hot forging and pressing, knurling, roll threading, shearing, spinning, swaging, and stamping.

Corrosion Resistance: Good to excellent. Susceptible to galvanic corrosion when coupled with iron, aluminum, magnesium, lead, tin, and zinc. Good resistance to atmospheric, brackish water, sea water, and non-oxidizing acid corrosion, but avoid heating in oxidizing atmospheres or exposing to oxidizing acids, moist halogens, sulfides, ammonia, or solutions with ammonium ions.

Forms: pipe, plate, rod, shapes, sheet, strip, tube, and wire.

UNS C10200 - ASTM (flat products) B48, B133, B152, B187, B272, B370, B432, B451, (pipe) B42, B188, (rod) B12, B49, B124,B133, B187, (tubing) B68, B75, B88, B111, B188, B280, B359, B372, B395, B447, (shapes) B124,B133, B187, (wire) B1, B2, B3, B33, B47, B116, B189, B246, B286, B298, B355; C103 (UK); CDA 102 OF; CEN CW009A; Cu/cl NF A53301 (France), ISO Cu-OF R1337; JIS C1020 H3100 - sheet, plate, C1020 H3140 - bar (Japan); QQ-C-576 (flat products), QQ-C-502 (rod, shapes); QQ-C-576 (tube); QQ-C-502, QQ-W-343, MIL-W-3318 (wire)

Key Words: AS 101A 1567 (Australia), OFHC, coining, coppersmithing, ASTM B1, B2, B3, B12, B33, B42, B47, B48, B49, B68, B75, B88, B111, B116, B124, B133, B152, B187, B188, B189, B246, B272, ASTM B286, B298, B355, B359, B370, B372, B395, B432, B451, B447, C103, CDA 102 OF, CEN CW009A, Cu/cl NF A53301, QQ-C-576, CDA 102 OF, C103, ISO Cu-OF R1337, CEN CW008A, OFHC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.90 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 75 - 90½ hard
 90 - 105full hard
Tensile Strength, Ultimate 215 - 254 MPasoft
 261 - 441 MPahard
Tensile Strength, Yield 49.0 - 78.0 MPa
@Strain 0.1 %
varies with temper and cold work.
Elongation at Break 35 - 55 %
Modulus of Elasticity 117 GPa
Poissons Ratio 0.31
Fatigue Strength 67.0 MPatest specimen: annealed 25 mm diam. Rod
Machinability 20 %Based on 100% machinability for BS2874 CZ 121 Free-machining brass (20% of 100% for UNS C360000)
Forgeability 65 %
Shear Modulus 44.0 GPa
Izod Impact 34.0 - 61.0 JType of Impact test unknown. Range reflects both soft and hard tempers.
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000169 - 0.00000173 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 17.0 µm/m-°C
@Temperature 20.0 - 100 °C
 17.3 µm/m-°C
@Temperature 20.0 - 200 °C
 17.7 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.385 J/g-°C
@Temperature 20.0 °C
Thermal Conductivity 383 - 391 W/m-K
@Temperature 20.0 °C
Melting Point 1083 °C
Annealing Point >= 700 °F
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu >= 99.95 %includes silver (minimum 99.95% Cu+Ag)

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Oxygen-free high conductivity Copper, Hard, UNS C10200
Oxygen-free electronic Copper, UNS C10100
Copper, Cu; Annealed
Oxygen-free Copper (OF), UNS C10200, H00 Temper, flat products
Copper, Cu; Cold Drawn

MC10200b1 / 10337

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.