MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Shanghai Potomer MBS-700 PVC Impact Modifier
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Brief Introduction: PVC Impact Modifier MBS-700 is the tercopolymer of methyl methacrylate(M), butadiene(B), styrene(S) , mainly used in the process of rigid PVC. The main characteristics of Impact Modifier MBS-700 is that it offers PVC products with high impact resistance, high transparency, good processability and reduced gelation time and less crease-whitening.

Properties: White amorphous powder with excellent chemical stability and thermoplasticity .

Applications(for transparent application): PVC Impact Modifier MBS-700 is mainly used in PVC film, sheet material, granular material, tubing for indoor use, pipe fittings, to improve their impact strength.

Information provided by Shanghai Potomer International Trade Co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.300 - 0.500 g/cc
Volatiles 1.0 %
Particle Mesh Size 20 Mesh0.98
 
Descriptive Properties
Color/AppearanceWhite powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSPOTOM198 / 284644

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.