MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Ganpati Exim MBT (M)
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Molecular Formula: C7H5NS2

Properties : Grayish-white or light yellow powder with slightly foul odor and bitter taste, non poisonous. Specific gravity: 1.42-1.52. Melting point : over 170o C. Easily soluble in ethyl acetone, acetone, dilute solution of sodium hydroxide and sodium carbonate, soluble in ethyl alcohol, not easily soluble in benzene, insoluble in water and gasoline,

Application: Accelerator M is a hemi-ultra accelerator of NR and SR, has wide range of vulcanization. It can be applied alone and together with dithicarbamates, thiuram type, guanidines and other alkaline accelerators. Mainly used in manufacture of rubber tires, belts, rubber shoes and other technical rubber goods.

Information provided by Ganpati Exim PVT. LTD.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.42 - 1.52 g/cc
Molecular Weight 167.26 g/mol
Ash <= 0.30 %
 
Thermal PropertiesOriginal ValueComments
Melting Point >= 171 °C
 
Descriptive Properties
Appearancegrayish-white or light yellow powder
Heating Loss<0.4%
Residue<0.1%150µm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGANPATI064 / 317348

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.