MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Milliken® GeoSpray™ Geopolymer Mortar
Categories: Other Engineering Material

Material Notes: GeoSpray™ geopolymer is a high performance fiber reinforced mortar specifically designed for structural rehabilitation. This high strength, ultra-low porosity material is made from natural mineral polymers and recycled industrial waste streams. GeoSpray is designed for use through multiple application techniques including pouring, placing, trowelling, spraying, or centrifugal casting. GeoSpray can be used for rehabilitation of pipes and structures in Civil Infrastructure, Gas & Oil and Chemical industries. In addition, it is used to repair tunnels, bridges, and roads as well as to rehabilitate buildings and containment areas.

Information provided by Milliken®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break >= 750 MPa
@Time 2.42e+6 sec
ASTM C496
Modulus of Elasticity 207 GPa
@Time 101000 sec
ASTM C469
 465 GPa
@Time 2.42e+6 sec
ASTM C469
Flexural Strength 8.30 MPa
@Time 86400 sec
ASTM C78
 9.00 MPa
@Time 2.42e+6 sec
ASTM C78
Compressive Strength >= 2.50 ksi
@Time 86400 sec
ASTM C39
 >= 8.00 ksi
@Time 2.42e+6 sec
ASTM C39
Adhesive Bond Strength >= 1300 psi
@Time 86400 sec
to Concrete; ASTM C882
 >= 2500 psi
@Time 2.42e+6 sec
to Concrete; ASTM C882
Abrasion 0.67
@# of Cycles 6.00 ,
Time 2.42e+6 sec
[%] Loss; ASTM C1138
 
Thermal PropertiesOriginal ValueComments
Shrinkage 0.070 %
@Time 2.42e+6 sec
ASTM C1090
 
Processing PropertiesOriginal ValueComments
Cure Time 60.0 - 75.0 minInitial Set; ASTM C807
 90.0 - 110 minFinal Set; ASTM C807

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Silicon Carbide, Alpha SiC
Solvay Thornel® P-100 Carbon Fiber/Epoxy Advanced Composite System
Morgan Advanced Ceramics Sintox™ Al (Porous) >99% Alumina
Morgan Advanced Ceramics Halsic RX (chemically doped) Silicon Carbide
Molybdenum Carbide, Mo2C

PMILLIK013 / 194984

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.