MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Momentive Performance Materials GE Sealants & Adhesives Supreme Silicone Window & Door Sealant
Categories: Polymer; Thermoset; Silicone

Material Notes: Supreme Silicone Window & Door sealant is a premium 100% silicone sealant with exceptional adhesion and flexibility. This sealant offers 50% joint movement capability and can withstand extreme expansion or contraction associated with wide temperature fluctuations. Ideal for a number of highly demanding exterior and interior projects, this durable sealant can be rain-ready in as little as 30 minutes, is resistant to UV degradation and has lifetime mold-free product protection. Supreme Silicone Window & Door sealant’s airtight and permanently waterproof seal helps keep weather out and reduce energy consumption. Backed by a lifetime guarantee.

Information provided by Momentive Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.02 g/ccCured.
Volatile Organic Compounds (VOC) Content <= 35 g/lUncured. Excluding water & exempt compounds; WPSTM C1454
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 19ASTM D2240
Tensile Strength 1.57 MPaASTM D412
Elongation at Break 483 %ASTM D412
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 400 °F
Minimum Service Temperature, Air -60.0 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 24.0 hourFull Cure
Tack-Free Time 30.0 min
@Temperature 22.2 °C
50% RH; ASTM C679
Working Life 6.00 - 12.0 min
 
Descriptive Properties
AppearancePaste
Carb Chem Curing VOC< 3.0 wt%
ColorClearM90016
 WhiteM90015
Consistency / Sag< 0.1 inchesASTM D2202
Joint Movement Capability±50%ASTM C719.
OdorLight Ammonia
Rain Ready30 minutes
UV & Weathering ResistanceExcellent30 yr study

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMOMEN9938 / 265749

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.