MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SABIC LNP™ THERMOCOMP™ Compound DX11354X Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP THERMOCOMP DX11354X compound is based on Polycarbonate (PC) resin containing proprietary fillers. Added features of this grade include: Improved Plating Surface and Mechanical Performance suitable for Laser Direct Structuring (LDS) applications, Improved Impact, Colorable.

Features: Enhanced Ductility,Laser Direct Structuring,Circuit Solution,Colorable

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.28 g/ccISO 1183
Moisture Absorption 0.0200 %Injection Molding
 0.0500 %23°C / 50% RH; ISO 62
Viscosity 20 cP
@Load 1.20 kg,
Temperature 300 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm24hrs; ISO 294
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm24hrs; ISO 294
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 45.0 MPa50 mm/min; ASTM D638
 51.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 54.0 MPa50 mm/min; ISO 527
 55.0 MPa50 mm/min; ASTM D638
Elongation at Break 70 %50 mm/min; ASTM D638
 84 %50 mm/min; ISO 527
Elongation at Yield 5.0 %50 mm/min; ASTM D638
 5.0 %50 mm/min; ISO 527
Tensile Modulus 2320 MPa1 mm/min; ISO 527
 2400 MPa50 mm/min; ASTM D638
Flexural Strength 86.0 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
 86.0 MPayield, 2 mm/min; ISO 178
Flexural Modulus 2380 MPa1.3 mm/min, 50 mm span; ASTM D790
 2450 MPa2 mm/min; ISO 178
Izod Impact Notched 700 JASTM D256
Izod Impact, Notched (ISO) 60.0 kJ/m²80*10*3; ISO 180/1A
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmASTM D257
Surface Resistance 1.00e+16 ohmASTM D257
Dielectric Constant 3.03
@Frequency 1e+9 Hz
ASTM D150
Dissipation Factor 0.0066
@Frequency 1e+9 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 65.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
CTE, linear, Transverse to Flow 71.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
Deflection Temperature at 1.8 MPa (264 psi) 117 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 121 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 136 °CRate A/50; ASTM D1525
 136 °CRate B/50; ISO 306
UL RTI, Electrical 80.0 °CUL 746B
UL RTI, Mechanical with Impact 80.0 °CUL 746B
UL RTI, Mechanical without Impact 80.0 °CUL 746B
Flammability, UL94 HB
@Thickness >=1.00 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 255 - 275 °C
Zone 2 260 - 280 °C
Zone 3 260 - 280 °C
Melt Temperature 260 - 280 °CInjection Molding
Mold Temperature 80.0 - 140 °C
Drying Temperature 110 - 120 °CInjection Molding
Dry Time 2.00 - 4.00 hourInjection Molding
Precipitation Temperature 40.0 - 60.0 °CHopper Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH81561 / 289508

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.