MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Chemlon® 100 HU Nylon 66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Heat Stabilized

Material Notes: Availability: Europe; Asia Pacific; North America

Additive: Heat Stabilizer; Lubricant; UV Stabilizer

Features: General Purpose; Good Processability; Good Toughness; Heat Stabilized; High Strength; Lubricated; UV Resistant

Uses: Appliances; Automotive Applications; Electrical/Electronic Applications

Form: Pellets

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccASTM D792
Water Absorption 1.2 %
@Time 86400 sec
ASTM D570
Maximum Moisture Content 0.20
Linear Mold Shrinkage, Flow 0.015 in/inASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 12000 psiASTM D638
Elongation at Break 25 %ASTM D638
Flexural Strength 16500 psiASTM D790
Flexural Modulus 425000 psiASTM D790
Izod Impact, Notched 1.00 ft-lb/inASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 190 °FUnannealed; ASTM D648
Flammability, UL94 V-2
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 540 °F
Middle Barrel Temperature 520 °F
Front Barrel Temperature 500 °F
Nozzle Temperature 500 °F
Melt Temperature 490 °F
Mold Temperature 70.0 - 200 °F
Drying Temperature 150 - 180 °F
Injection Pressure 5000 - 20000 psi
Screw Speed 60 - 120 rpm
 
Descriptive Properties
AppearanceGrey

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ0424 / 236915

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.