ATOFINA Propylene 13712 is a nucleated antistatic heterophasic copolymer. PPC 13442 is characterized by good stiffness and impact resistance as well as low shrinkage and low warpage. It has been formulated for excellent antistatic properties.
ATOFINA Propylene PPC 13442 has been developed for high speed injection molding of thin walled packaging containers and household articles. Information provided provided by Total Petrochemicals. Total Petrochemicals includes former Fina and Atofina plastics product lines. |