MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hexcel® HexPly® M9.6H Epoxy Resin Matrix
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: HexPly® M9.6H is a hotmelt, thermosetting, moderate tack epoxy resin matrix, specifically designed for prepreg applications at which short cure cycles of 100°C and above are required. M9.6H can be used for manufacture of large industrial components, suitable for cure of thin and thick sections. M9.6H exhibits a long out-life at ambient conditions.

Information provided by Hexcel Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.10 - 1.22 g/cc
Viscosity 100 cP
@Temperature 105 °C
Dynamic Complex Viscosity of HexPly® M9.6GF @2°C/min
 1000 cP
@Temperature 121 °C
Dynamic Complex Viscosity of HexPly® M9.6GF @2°C/min
 100000 cP
@Temperature 40.0 °C
Dynamic Complex Viscosity of HexPly® M9.6GF @2°C/min
 1.00e+6 cP
@Temperature 130 °C
Dynamic Complex Viscosity of HexPly® M9.6GF @2°C/min
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 105 - 115 °CTypical cured, following a 30min cure @120°C
 120 - 130 °COptimum cured, following a 120min cure @120°C
 
Processing PropertiesOriginal ValueComments
Cure Time 0.500 hour
@Temperature 120 °C
+/-7min
 0.750 hour
@Temperature 110 °C
+/-10min
 1.167 hour
@Temperature 100 °C
+/-15min
Shelf Life 2.00 Month
@Temperature 23.0 °C
 6.00 Month
@Temperature 5.00 °C
 18.0 Month
@Temperature -18.0 °C
 
Descriptive Properties
ColorOff white - Yellowish

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHEXCB9132 / 322288

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.