MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

(Viewing data as-entered. Click here to return)
Indium Corp. 1075-EXR 40 VOC-Free Wave Solder Flux
Categories: Fluid; Metal; Nonferrous Metal; Solder/Braze Alloy

Material Notes: 1075-EXR 40 VOC-free, is a non-halide, synthetic resin flux specifically developed for wave soldering, surface mount, mixed technology and through-hole electronic assemblies.
1075-EXR 40 is a water-based, non-flammable formulation, that eliminates special storage requirements and reduces VOC emissions.
1075-EXR 40 is formulated to reduce solder balling and provide excellent solderability on difficult to solder assemblies.

Features

  • Excellent Surface Wetting
  • Eliminates Cleaning
  • VOC-Free formulation
  • Reduces Solder Balling
  • Increased Activity
  • Conforms to Telecordia GR-78 Specification

Physical Properties

  • Color: Clear
  • Flash Point: None
  • Flux Type: ORL0

Information Provided by Indium Corporation

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.019 g/cc
@Temperature 25.0 °C
 1.019 g/cc
@Temperature 15.5 °C
Solids Content 5.0 %
 
Chemical PropertiesOriginal ValueComments
Acid Value 40
 
Electrical PropertiesOriginal ValueComments
Insulation Resistance 6.76e+11 ohmTelcordia, Control - final reading; IPC B25A
 8.33e+11 ohmTelcordia, Control - initial reading; IPC B25A
 
Descriptive Properties
Flash PointNone

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Indium Corp. 1075-EXR 44 Wave Solder Flux
Indium Corp. 1075-EXR 30 VOC-Free Wave Solder Flux
Indium Corp. 1075-EX VOC-Free Wave Solder Flux
Indium Corp. 1075-EX 30 VOC-Free Wave Solder Flux
Indium Corp. 1075 Wave Solder Flux VOC-Free

NNIN961 / 131600

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.