MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Rogers Arlon Ultrapad™ D 65 (55073R062) 0.0622 (1.58 mm) Cured Silicone Rubber with Fiberglass Substrate
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Silicone, Molded, Glass Fiber Filled

Material Notes: Description: Ultrapad™ D65 Silicone-based press pad. Arlon UltraPad press pad is a high performance, fiberglass reinforced, silicone sheet designed for flex and rigid-flex circuitry lamination. UltraPad press pad provides excellent pressure uniformity with good consistency and longevity throughout its service life. UltraPad press pads are the most cost effective press pad solution across a wide range of process pressures and temperatures.

Design/Construction:
Interleave: Polyethylene
Side 1: Cured Silicone Rubber
Substrate: Style 162 Fiberglass
Side 2: Cured Silicone Rubber

Advantages:
Consistent, reliable service life - predictable changeover schedule, higher yield (no lost loads)
Uniform pressure over the entire laminate surface - higher yield, better quality laminate
Available in softer low durometer variants - lower durometer > better pressure uniformity

Product Use: Press Pad

Appearance: Red silicone rubber on fiberglass cloth

This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.

Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.09 g/ccSilicone Property; Arlon SQA-TMS-024
Thickness 2.95 milInterleave
 18.9 milSubstrate; Arlon SQA-TMS-003
 21.7 milSide 2; Arlon SQA-TMS-003
 21.7 milSide 1; Arlon SQA-TMS-003
 62.2 milOverall; Arlon SQA-TMS-003
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 43Silicone Property; ASTM D2240
 65Product Property; ASTM D2240
Tensile Strength 1130 psiSilicone Property; ASTM D412
Elongation at Break 854 %Silicone Property; ASTM D412
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 572 °F
 
Processing PropertiesOriginal ValueComments
Shelf Life 60.0 Month
@Temperature 23.0 °C
From date of manufacture
 
Descriptive Properties
ColorNaturally WhiteSubstrate
 Red
Recommended Application Pressure0 - 5 Mpa
Service Life(200°C and 2.07MPa)
 (225°C and 2.07MPa)
 (250°C and 2.07MPa)
Total Product Weight (g/m2)1605Arlon SQA-TMS-025

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay Vac-Pak® UHT750 Vacuum bagging film
Solvay EF2000 Organosilicate Polymer
Rogers Arlon 51073R031 0.0311" (0.79 mm) Cured Silicone Rubber with Fiberglass Substrate
Manifattura Cattaneo VESPEL® SP1 Polyimide
Hexcel® HexForce™ 328 Aramid Fabric

PARL334 / 125520

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.