MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Vibrantz Technologies CF 7586 Low-Temperature Sealing
Categories: Ceramic; Glass

Material Notes: DEVITRIFYING
Typical Powder Form: TF

Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet specific thermal expansion requirements. Uses include hermetic and compression sealing of IC packages, plasma displays, CRTs, ferrites, fiber optics, as well as other ceramic, metal and glass substrate materials.

Information provided by Ferro Corporation

Ferro Corporation is now a part of Vibrantz Technologies.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 5.04 g/cc
Particle Size 10 - 16 µm50% of particles
 <= 75 µm
 
Mechanical PropertiesOriginal ValueComments
Heat Seal Strength Initiation Temperature 600 °C30 min
 
Thermal PropertiesOriginal ValueComments
CTE, linear 6.20 µm/m-°Cat Set Pt. (Fired Thermal Expansion)
 6.00 µm/m-°C
@Temperature 260 °C
Fired Thermal Expansion
Softening Point 513 °C
Annealing Point 430 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Schott D 263® T eco Ultra-Thin Glass
Vibrantz Technologies F 2719 Metal Sealing
A. Schulman Gapex® RPP20EU38BK 20% Fiberglass Reinforced, Chemically-Coupled, Impact-Modified Polypropylene
A. Schulman Gapex® APP40GR30HB 40% Fiberglass/Mineral Reinforced, Chemically-Coupled, Homopolymer Polypropylene
Vibrantz Technologies EG 2012 Low-Temperature Sealing

CFERR29 / 843

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.