MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Reltek BONDiT™ HM-502 Coating, Sealant, Adhesive System
Categories: Polymer; Adhesive

Material Notes: A protective coat for most metal, glass, and ceramic materials for use against corrosion and other chemical attacks. Useful against fungi growth. Bondit HM-502 is a thermoplastic emulsion system.

Information provided by Reltek LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.955 g/cc
Moisture Absorption at Equilibrium 0.040 %
@Temperature 40.0 °C
100% RH
Water Vapor Transmission <= 2.30 g/100 in²/day
@Temperature 38.0 °C
ASTM E-96
Oxygen Transmission 350 cc-mil/100 in²-24hr-atm
@Temperature 23.0 °C
ASTM D1434
Viscosity 850 cP
Environmental Stress Crack Resistance >= 200 hour
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 42ASTM D2240
Tensile Strength at Break 900 psiASTM D638
Elongation at Break 350 %ASTM D638
2% Secant Modulus 3200 psiASTM D790
 
Thermal PropertiesOriginal ValueComments
Crystallization Temperature 75.0 °C
Brittleness Temperature -23.0 °CASTM D746
 
Descriptive Properties
Approximate reverse impact24
ColorClear
Fungi ResistanceNo Growth
Insulation Resistance (V/mil)500
Thermal ShockNo effect

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Elantas EN-8 (Conap) Casting, Potting, and Molding Compound
Valley Adhesives EM-500 High Temperature Application Glue Stick
Sika SikaTack® UltraFast Fast Cure One Part Polyurethane Adhesive
Reltek BONDiT™ B-4682 Adhesive, Sealant & Coating System
Overview of materials for Thermoset Polyurethane, Adhesive

PAQREL35 / 79999

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.