MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Nanosonic Metal Rubber™
Categories: Metal; Polymer

Material Notes: Metal Rubber™ is a unique self-assembled nanocomposite material that combines the high electrical conductivity of metals with the low mechanical modulus of elastomers. Self-assembly processing allows the simultaneous modification of both conductivity and modulus during manufacturing.

Metal Rubber™ has a wide range of possible applications, from mechanically flexible electrical interconnections and electromagnetic shielding to the measurement of large mechanical deformations.

Material maintains its shape and remains electrically conductive, even after millions of cycles at nominal strain. Even after large cyclic strains up to 200%, material resists wrinkling and failing from deformation.

Information provided by Nanosonic, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Elongation at Break 200 - 300 %
Modulus of Elasticity 0.0100 GPa
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 0.10 - 100 ohm
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 170 °C
Minimum Service Temperature, Air -60.0 °C
Glass Transition Temp, Tg -60.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sandvik Bioline High-N Tube and pipe, seamless
Polyram PlusTek PB202G50BK39 Nylon 6, 50% Glass Fiber Reinforced, UV and Heat Stabilized
Overview of materials for Polyester Thermoplastic Elastomer
Network Polymers Softflex® 0470
Epoxy Technology EPO-TEK® OG133-8 UV Cure Optical Epoxy

PNANO000 / 54708

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.