MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Evonik VESTAKEEP® I4 R PEEK
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Unreinforced

Material Notes: VESTAKEEP® i4 R are rods based on implantable grade VESTAKEEP® i4 G resin.

Information provided by Evonik

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.30 g/ccISO 1183
Moisture Absorption 0.12 %50% RH; ISO 62
Water Absorption at Saturation 0.50 %ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break >= 100 MPaISO 527-1
Tensile Strength, Yield 109 MPaISO 527-1
Elongation at Break >= 20 %ISO 527-1
Elongation at Yield 4.8 %ISO 527-1
Tensile Modulus 4000 MPaYoung's; ISO 527-1
Flexural Strength 165 MPaISO 178
Flexural Modulus 4.05 GPaISO 178
Izod Impact, Notched (ISO) 5.50 kJ/m²ISO 180
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.8
@Frequency 50 Hz
IEC 60250
 2.8
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 21.0 kV/mmK20/K20; IEC 60243-1
 
Thermal PropertiesOriginal ValueComments
Melting Point 340 °CISO 11357
Crystallization Temperature 285 °CRecrystallization; ISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 160 °CISO 75-1
Glass Transition Temp, Tg 145 °Con set; ISO 11357
 155 °Cmidpoint; ISO 11357

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik VESTAKEEP® 4000CF30 PEEK
Evonik VESTAKEEP® 4000GF30 PEEK
VICTREX™ PEEK 90HMF40 Polyetheretherketone (PEEK), 40% Carbon Fiber Reinforced
Evonik VESTAKEEP® 2000FP PEEK
Evonik VESTAKEEP® 2000P PEEK

PEVONIL223 / 196427

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.