MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Conventus Polymers DuraPEEK 1000SHF PEEK
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Unreinforced

Material Notes: DURAPEEK 1000SHF is a super high flow grade of PEEK. It is an equivalent to Victrex 90G, and Evonik 1000G. It is natural in color. It is available in North America, Europe, and Pacific.

Information provided by Conventus Polymers LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.30 g/ccISO 1183
Melt Flow 182 g/10 min
@Load 5.00 kg,
Temperature 380 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Stress 105 MPaISO 527-2
Elongation at Break 10 %ISO 527-2
Tensile Modulus 551000 psiISO 527-2
Charpy Impact Unnotched 60.9 kJ/m²ISO 179
Charpy Impact, Notched 5.04 kJ/m²ISO 179
 
Thermal PropertiesOriginal ValueComments
Melting Point 340 °CISO 11357-3
Vicat Softening Point 635 °FISO 306/A
Flammability, UL94 V-0
@Thickness 1.52 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCONV789 / 265869

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.