MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Daikin DAI-EL® LT-303L Fluoroelastomer Terpolymer, 65% Fluorine Content
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: DAI-EL® LT-303L is a terpolymer suitable for various peroxide cure systems. LT-303L can be formulated to eliminate the post cure process. LT-303L is designed for injection molding applications that require good low temperature flexibility and high elongation.

Typical Applications: O-Rings, gaskets, seals

Rheological Properties:
Temperature: 177°C
Frequency: 100 cpm
Strain: 0.5°
Test time: 6 min

Information provided by Daikin.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.79 g/cc
Mooney Viscosity 14
@Temperature 121 °C
ML 1+10
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 71
Tensile Strength at Break 20.1 MPa
Elongation at Break 250 %
100% Modulus 4.40 MPa
@Strain 100 %
Compression Set 14 %
@Temperature 175 °C,
Time 252000 sec
#214 O-ring; ASTM D395 Method B
 27 %
@Temperature 200 °C,
Time 252000 sec
#214 O-ring; ASTM D395 Method B
 
Thermal PropertiesOriginal ValueComments
Minimum Service Temperature, Air -32.0 °CLow Temperature Retraction, TR10
 
Processing PropertiesOriginal ValueComments
Cure Time 0.400 mints2, scorch time, MDR 2000
 0.500 mint'50, time to 50% cure, MDR 2000
 0.700 mint'90, time to 90% cure, MDR 2000
 4.00 hour
@Temperature 200 °C
Post cure
 10.0 min
@Temperature 177 °C
Press Cure
 
Component Elements PropertiesOriginal ValueComments
Fluorine, F 65 %
 
Descriptive Properties
ColorWhite to light pink
MH27.8 dNmmaximum torque, MDR 2000
ML0.2 dNmminimum torque, MDR 2000
Test Formula100 phrDAI-EL® LT-303L
 3 phrPeroxide (50% Activity)
 3 phrZinc Oxide
 30 phrMT Carbon Black (N-990)
 4 phrTAIC (72% Activity)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ametek Ultra 303L P/M Stainless Steel, Sintered from 6.0 g/cc Green Density
Ametek Ultra 303L P/M Stainless Steel, Sintered from 6.65 g/cc Green Density
Ametek Ultra 303L P/M Stainless Steel, Sintered from 6.35 g/cc Green Density
AISI Type 304L Stainless Steel
AISI Type 302B Stainless Steel, annealed sheet

PDAIJ9865 / 209936

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.