High-strength Steel Comments: Docol BH - Cold Rolled Steel - rephosphorized steel with bake hardening effect. Property values are for cold-rolled steel; thicknesses 0.40 - 2.0 mm. Iron content is approximate - exact composition is not reported by the manufacturer. Data provided by SSAB Tunnplat. |