MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Hostalen GM9350C BLACK High Density Polyethylene (HDPE), Injection Molded
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: Hostalen GM9350C BLACK is a compounded high molecular weight high density polyethylene. Typical customer applications include fuel tank filler pipes requiring electrical conductivity. It is supplied in pellets and is stabilized with antioxidants for the extrusion process. The product features a very good Environmental Stress Cracking Resistance (ESCR) and a good chemical resistance. Typical processes include blow molding and injection molding. Hostalen GM9350C BLACK is not intended for use in medical and pharmaceutical applications. The product can not be used for food contact applications. Applications: Fuel Tanks

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 34.3 lb/ft³
Density 0.995 g/ccISO 1183-1
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 28.0 MPaISO 527-1,-2
Elongation at Yield 7.0 %ISO 527-1,-2
Tensile Modulus 1200 MPaISO 527-1,-2
Charpy Impact, Notched 2.50 kJ/m²
@Temperature -30.0 °C
ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1e+05IEC 93
Surface Resistivity per Square 10000 ohmIEC 93
 
Processing PropertiesOriginal ValueComments
Processing Temperature 180 - 230 °CExtrusion Temperature/blow molding
 240 - 270 °CInjection Molding Temperature
 
Descriptive Properties
Processing Methodinjection molding, extrusion blow molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Hostalen ACP 5331H High Density Polyethylene (HDPE), Injection Molded
LyondellBasell Hostalen ACP 6541A UV High Density Polyethylene (HDPE), Injection Molded
LyondellBasell Hostalen GC 7258 High Density Polyethylene (HDPE), Injection Molded
LyondellBasell Hostalen GC 7260 LS High Density Polyethylene (HDPE), Injection Molded
LyondellBasell Hostalen 5231H High Density Polyethylene (HDPE), Injection Molded

PEQT8497 / 220132

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.