MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Phillips 66 Syncon® AW Hydraulic Fluid ISO Grade 32
Categories: Fluid; Lubricant; Polyalphaolefin (PAO)

Material Notes: Phillips 66® Syncon AW Hydraulic Fluid is a premium quality, synthetic anti-wear hydraulic fluid developed for use in industrial and mobile equipment operating at extreme temperatures. It is particularly recommended for use in applications where operating conditions may be unfavorable or too severe for conventional mineral oil-based hydraulic oils. Syncon AW Hydraulic Fluid is formulated with synthetic polyalphaolefin (PAO) base oils and an ashless (zinc-free) additive package to provide excellent performance over a wide temperature range. It provides excellent wear protection for hydraulic pumps and motors, and protects hydraulic system components against rust and corrosion. It has outstanding oxidation resistance and thermal stability at high temperatures to minimize deposit formation and provide long service life. It also has excellent low-temperature properties for cold start-ups. It has excellent water-separating properties to minimize the formation of emulsions, and is resistant to excessive foaming that can cause poor or sluggish hydraulic system response. It has a high dielectric strength for use as an insulating oil in electrical service bucket trucks. Syncon AW Hydraulic Fluid meets the performance requirements of all major hydraulic pump manufacturers, and is recommended for use in all types of high pressure, high-speed hydraulic pumps.

Applications:

  • Industrial and mobile equipment operating under extreme-temperature conditions
  • Automated machine tools
  • Bucket trucks (cherry pickers) used for servicing electrical power lines or for tree trimming
  • Hydraulic hoists and service station lifts
  • Mobile construction equipment
  • Chain drives
  • Electric motor bearings
Syncon AW Hydraulic Fluid meets the requirements of the following industry specifications:
  • DIN 51524 Part 2, Anti-wear Hydraulic Oils, Type HLP
  • ISO 11158:1997, Family H (Hydraulic Systems), Type HM
  • U. S. Steel 127
Features/Benefits:
  • Outstanding oxidation resistance and thermal stability at high temperatures
  • Outstanding pumpability at low temperatures
  • Excellent wear protection for hydraulic pumps and motors
  • Protects against rust and corrosion
  • Separates rapidly from water
  • Good foam resistance
  • High dielectric strength
  • Compatible with conventional mineral oils and commonly used seals

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.853 g/cc
Density 7.10 lb/gal
Viscosity Measurement 125Index
Saybolt Viscosity at 100°F 164 SUS
Saybolt Viscosity at 210°F 45.7 SUS
Kinematic Viscosity at 40°C (104°F) 32 cSt
Kinematic Viscosity at 100°C (212°F) 5.8 cSt
Oxidative Stability 33.3 hourRPVOT; ASTM D2272
ASTM Color 0.50ASTM D1500
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 0.17[mg KOH/g]; ASTM D974
 
Mechanical PropertiesOriginal ValueComments
Four Ball Wear 0.470 mmScar Diameter; ASTM D4172
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 35.0 kV/mmASTM D877
 
Thermal PropertiesOriginal ValueComments
Pour Point -60.0 °C
Flash Point 240 °CCOC
 
Descriptive Properties
Copper Corrosion1aASTM D130, 48 hrs @ 80°C
Demulsibility10 minutes to passASTM D1401
FZG Scuffing Test12 failure load stageASTM D5182

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON5430 / 198683

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.