MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Extreme Materials from MCAM
Visit Mitsubishi Chemical Advanced Materials for Extreme Materials - high performance plastic machining stock engineered to replace metals such as nickel alloys or stainless steel.

(Viewing data as-entered. Click here to return)
Special Metals MONEL® Alloy 450  (discontinued **)
Categories: Metal; Nonferrous Metal; Copper Alloy; Nickel Alloy; Superalloy

Material Notes: A copper-nickel alloy of the 70-30 type having superior weldability. It is resistant to corrosion and bio-fouling in sea water, has good fatigue strength, and has relatively high thermal conductivity. Used for sea-water condensers, condenser plates, distiller tubes, evaporator and heat exchanger tubes, and salt-water piping. Standard product forms are round, hexagon, flats, forging stock, pipe, tube, plate, sheet, and wire.

Data provided by the manufacturer, Special Metals.

Key Words: ASME SB-111, SB-171, SB-359, SB-395, SB-466, SB-467, SB-543, Boiler Code Sections III, IV, VIII, IX; SAE J461, J463, MIL-T-15005, MIL-C-15726, MIL-T-16420, MIL-T-22214, Monel Nickel-Copper Alloy, UNS C71500; CDA 715; ASTM B 111, B 122, B 151, B 171, B 359, B 395, B 432, B 466, B 467, B 543, B 552
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.91 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 385 MPaAnnealed
 280 MPa
@Temperature 425 °C
Annealed prior to test
Tensile Strength, Yield 165 MPaAnnealed
 100 MPa
@Temperature 425 °C
Annealed prior to test
Elongation at Break 56 %Annealed prior to test.
 40 %
@Temperature 425 °C
Annealed prior to test.
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000412 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 15.5 µm/m-°C
@Temperature 20.0 - 100 °C
Specific Heat Capacity 0.380 J/g-°C
Thermal Conductivity 29.4 W/m-K
Melting Point 1170 - 1240 °C
Solidus 1170 °C
Liquidus 1240 °C
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 66 %As remainder
Iron, Fe 0.40 - 1.0 %
Lead, Pb <= 0.050 %
Manganese, Mn <= 1.0 %
Nickel, Ni 29 - 33 %Including Cobalt
Phosphorus, P <= 0.020 %
Sulfur, S <= 0.020 %
Zinc, Zn <= 1.0 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Special Metals MONEL® Alloy 400
Special Metals MONEL® Alloy K-500
Special Metals MONEL® Alloy 401
Special Metals MONEL® Alloy R-405
Special Metals MONEL® 404 Copper-Nickel Alloy

NINC13 / 17396

Metalmen Sales

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.