MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Lanxess Mesamoll® 51067 Plastic Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Mesamoll® 51067 is a general purpose plasticizer with good gelling behavior. The trial product is compatible with many types of polymers including PVC and polyurethanes.

Chemical composition: mixture of alkylsulfonic phenyl ester (ASE)

CAS Reg. No: 91082-17-6 (ASE)

General Mesamoll® 51067 is characterized by

  • an excellent compatibility with a large number of polymers including PVC.
  • an outstanding gelling behavior in a PVC plastisol which provides the option of reducing processing temperatures or shorten processing times.
Applications: Mesamoll® 51067 can be used as a plasticizer for a wide range of articles based on polyvinyl chloride (PVC), polyurethane (PU), and natural and synthetic rubbers.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.07 g/ccDIN 51 757
Water Absorption <= 0.060 %DIN 51 777
Viscosity 70 cPDIN 53 015
 
Thermal PropertiesOriginal ValueComments
Pour Point -38.0 °FISO 3016
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.49DIN EN ISO 6320
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
 
Descriptive Properties
Color<350Hazen, DIN ISO 6271
Specifications119°CDissolution temp, DIN 53 408

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLANY8902 / 209294

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.