MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
EMS-Grivory Grilamid® L 25 nat Nylon 12, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Food Contact Acceptable; High Viscosity

Uses: Cast Film; Consumer Applications; Film; Medical Devices; Medical/Healthcare Applications; Non-oriented Film; Packaging

Agency Ratings: EU Food Contact; FDA Food Contact; USP Class VI

RoSH Compliance: RoSH Compliant

Automotive Specifications: ASTM D4066 PA423 Color: 6086 Natural; FOOD WSK-M4D739-A; GM QK 004422 Color: Natural

Appearance: Natural Color

Forms: Granules

Processing Method: Cast Film; Film Extrusion; Extrusion; Injection Molding

Information provided by EMS-Grivory

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.01 g/ccISO 1183
Water Absorption 0.70 %Equilibrium, 50% RH; ISO 62
Water Absorption at Saturation 1.5 %ISO 62
Water Vapor Transmission 0.520 g/100 in²/day85% RH; DIS 15106-1/-2
Oxygen Transmission 350 cc-mm/m²-24hr-atm0% RH; DIS 15105-1/-2
 370 cc-mm/m²-24hr-atm85% RH; DIS 15105-1/-2
Carbon Dioxide Transmission 1500 cc-mm/m²-24hr-atm0% RH; DIS 15105-1/-2
 1600 cc-mm/m²-24hr-atm85% RH; DIS 15105-1/-2
Melt Flow 20 g/10 min
@Load 5.00 kg,
Temperature 275 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 7250 psiISO 527-2
Film Tensile Strength at Yield, MD 5080 psiISO 527-3
Film Tensile Strength at Yield, TD 5080 psiISO 527-3
Tensile Strength, Yield 6530 psiISO 527-2
Film Elongation at Break, MD 850 %ISO 527-3
Film Elongation at Break, TD 900 %ISO 527-3
Film Elongation at Yield, MD 6.0 %ISO 527-3
Film Elongation at Yield, TD 6.0 %ISO 527-3
Elongation at Break >= 50 %Nominal; ISO 527-2
Elongation at Yield 10 %ISO 527-2
Tensile Modulus 203000 psiISO 527-1
Charpy Impact Unnotched NB
@Temperature 22.8 °C
ISO 179/1eU
 NB
@Temperature -30.0 °C
ISO 179/1eU
Tear Strength Test 114[lbf/in], Trouser, MD; ISO 6383-1
 143[lbf/in], Trouser, TD; ISO 6383-1
Elmendorf Tear Strength MD 998 gISO 6383-2
Elmendorf Tear Strength TD 998 gISO 6383-2
Film Tensile Strength at Break, MD 11600 psiISO 527-3
Film Tensile Strength at Break, TD 10200 psiISO 527-3
 
Thermal PropertiesOriginal ValueComments
Melting Point 352 °F10ºC/min; ISO 11357-3
Maximum Service Temperature, Air 302 °F
 
Optical PropertiesOriginal ValueComments
Gloss 150 %60°; ISO 2813
 
Descriptive Properties
Gelboflextest1300 holes/m2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGRIM084 / 307443

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.