MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Nouryon Duomeen CD Coco propylene diamine
Categories: Other Engineering Material

Material Notes: Duomeen CD is a coco propylene diamine.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.796 g/cc
@Temperature 80.0 °C
 0.803 g/cc
@Temperature 70.0 °C
 0.810 g/cc
@Temperature 60.0 °C
 0.824 g/cc
@Temperature 40.0 °C
 0.836 g/cc
@Temperature 25.0 °C
pH <= 10
Viscosity 58 cP
Vapor Pressure 0.000130 bar
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.595 BTU/lb-°F
@Temperature 37.8 °C
 0.612 BTU/lb-°F
@Temperature 60.0 °C
Melting Point 15.0 °C
Boiling Point >= 300 °C
@Pressure 0.101325 MPa
Pour Point 21.0 °C
Flash Point >= 150 °C
 
Optical PropertiesOriginal ValueComments
Gardner Color Number 0.00 - 2.0
 
Component Elements PropertiesOriginal ValueComments
H2O, Water <= 2.0 %
 
Descriptive Properties
Amine number409-442 mg KOH/g
AppearanceLiquid
Cloud point23°C
Content= 45 %Primary Amine
 = 45 %Secondary Amine
 0-12 g I2/100 gIodine value
 127-137 g/eqNeutralization equivalent
Equivalent mass132 g/eq
HLB17.5Davies Scale 0-40

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNOURY491 / 286014

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.