MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Hot Pour Ladles and Ladle Liner
Categories: Ceramic; Oxide

Material Notes: Vacuum formed products are rigid, self-supporting fiber insulation manufactured from a slurry of ceramic fibers, binders and other proprietary ingredients. Customers are provided with optimized, engineered solutions from our wide range of formulations. These include hand-pouring ladles, sampling ladles, and ladle liners. Vacuum formed products, which are both compressed and bonded, have significantly greater density than non-bonded ceramic fiber. As a result, they are 33% more efficient than non-bonded fiber. Heat flow through vacuum formed fiber is greatly reduced leading to more onsistent metal contact. When these characteristics are considered in terms of ladles and ladle liners, these products offer definite advantages over typical ladles and ladle liners on the market. For hot pour ladles used exclusively in the aluminum market, where maximum protection against ontamination of critical alloys is required, the Alfibond® formulation is strongly recommended. Alfibond is an alumiphobic material with exceptional resistance to chemical deterioration by molten aluminum. Alumiphobic describes Alfibond’s lack of affinity or aversion to molten aluminum.

Information provided by Morgan Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CMORF6488 / 203272

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.