MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Domo TECHNYL® A 218 V25 Black 21NHFE PA66, 25% glass fiber, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Description: Polyamide 66, offering high flowability and productivity gains, reinforced with 25% of glass fiber, heat stabilized, for injection molding.

Available in: Europe

Product Applications: TECHNYL A 218 V25 BLACK 21NHFE is characterized by a high flowability and offers an excellent combination between thermal and mechanical properties. This grade is a perfect fit for the pulley application and gives very low rugosity levels. This grade improves the surface aspect and reduce the warpage of the parts. In the automotive industry, this Technyl grade definitely meets the requirements for engine components, such as: inlet manifold, air ducts - engine covers, pulleys and various housings and liquid containers. This product is available in black

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.32 g/ccISO 1183/A
Water Absorption 0.90 %
@Temperature 23.0 °C,
Time 86400 sec
ISO 62
Linear Mold Shrinkage 0.0071 cm/cmIsotropy
Linear Mold Shrinkage, Flow 0.0060 cm/cm
Linear Mold Shrinkage, Transverse 0.0085 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 150 MPaISO 527 Type 1A
Elongation at Break 2.7 %ISO 527 Type 1A
Tensile Modulus 8800 MPaISO 527 Type 1A
Charpy Impact Unnotched 55.0 kJ/m²ISO 179/1eU
Charpy Impact, Notched 8.00 kJ/m²ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 263 °CISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 255 °CISO 75/Af
 
Processing PropertiesOriginal ValueComments
Feed Temperature 270 - 275 °C
Front Barrel Temperature 285 - 290 °C
Mold Temperature 60.0 - 80.0 °C
Drying Temperature 80.0 °C
Moisture Content <= 0.20 %
 
Descriptive Properties
Compression Zone280-285°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PRHOD628 / 137859

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.