MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Nickel Silver, UNS C76200, OS050 Temper, Flat Products
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Nominal Grain Size 0.050 mm

Fabrication Properties: Excellent Suitability – Soldering, Brazing, Capacity for Being Cold Worked; Good Suitability – Oxyacetylene Welding, Spot Weld, Butt Weld; Fair Suitability – Gas Shielded Arc Welding, Seam Weld; Poor Suitability – Capacity for Being Hot Formed

Typical uses: Rheostats; Springs for Relays; Condensers

Applicable Specifications: Bar – ASTM B122/B122M; Plate - ASTM B122/B122M; Sheet – ASTM B122/B122M; Strip – ASTM B122/B122M, ASTM B888/B88M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.310 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 55.0 ksi
Tensile Strength, Yield 30.0 ksi0.2% Offset
Elongation at Break 42 %
Tensile Modulus 18000 ksi
Modulus of Rigidity 6800 ksi
Poissons Ratio 0.32Calculated
Machinability 20 %
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000190 ohm-cm9% IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.00 µin/in-°F
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.0900 BTU/lb-°F
Thermal Conductivity 26.0 BTU-in/hr-ft²-°F
Melting Point 1800 - 1880 °F
Solidus 1800 °F
Liquidus 1880 °F
Annealing Point 1000 - 1350 °F
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 57 - 61 %
Iron, Fe <= 0.25 %
Lead, Pb <= 0.090 %
Manganese, Mn <= 0.50 %
Nickel, Ni 11 - 13.5 %
Zinc, Zn 24.7 - 32 %As Balance

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC76200x7 / 293129

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.