MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Zotefoams Evazote® VA80 Ethylene Vinyl Acetate Copolymer Foam
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outstanding physical attributes.

Information provided by Zotefoams

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.0630 - 0.0850 g/ccsheet density
 0.0800 g/ccNominal skin/skin; BS ISO 7214 1998
Cell Length 0.730 mmTypical Diameter
 0.500 - 1.00 mm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore OO 6210 mm cell/cell thickness; ISO 868 1985
Tensile Strength 0.895 MPaISO 7214 1998
Elongation at Break 215 %
Compressive Yield Strength 0.0840 MPa
@Strain 10 %
BS ISO 7214 1998
 0.105 MPa
@Strain 25 %
BS ISO 7214 1998
 0.142 MPa
@Strain 40 %
BS ISO 7214 1998
 0.184 MPa
@Strain 50 %
BS ISO 7214 1998
Tear Strength 1.97 kN/mBS EN ISO 8067 1995
Compression Set 2.0 %
@Time 79200 sec,
Strain 25 %
24 hr recovery; BS ISO 7214 1998
 5.0 %
@Time 79200 sec,
Strain 25 %
0.5 hr recovery; BS ISO 7214 1998
 5.0 %
@Time 79200 sec,
Strain 50 %
24 hr recovery; BS ISO 7214 1998
 13 %
@Time 79200 sec,
Strain 50 %
0.5 hr recovery; BS ISO 7214 1998
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 85.0 °C
Minimum Service Temperature, Air -70.0 °C
Flammability Test 0.33
@Thickness 5.00 mm
Horizontal Burn Rate, mm/sec; ISO 7214 1998
 0.36
@Thickness 13.0 mm
Horizontal Burn Rate, mm/sec; ISO 7214 1998
 
Descriptive Properties
FlammabilityAutomotive: FMVSS.302 burn ratePass: 3mm and thicker

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PZOTEF951 / 150707

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.