MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
LyondellBasell Hostalen PP W2080 Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Hostalen PP W2080 is a natural homopolymer polypropylene with high fluidity and suitable for injection molding applications and as base resin for compounding applications. The product combines good stiffness with good impact strength and good dimensional stability of the final items. Hostalen PP W2080 is typically used to produce items by injection molding with long flow paths as well as with added recipes containing long/medium glass fiber (GMT/LFT). It is not intended for medical and pharmaceutical applications. Applications: Industrial

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccISO 1183-1
Melt Flow 50 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 80.0 MPaISO 2039-1
Tensile Strength, Yield 30.0 MPaISO 527-1,-2
Elongation at Yield 9.0 %ISO 527-1,-2
Tensile Modulus 1350 MPaISO 527-1,-2
Izod Impact, Notched (ISO) 1.50 kJ/m²
@Temperature 23.0 °C
ISO 180
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °Cunannealed; ISO 75B-1,-2
Vicat Softening Point 90.0 °CB50; ISO 306
 154 °CA50; ISO 306
DSC Induction Temperature 163 °CDSC
 
Descriptive Properties
Ball Indentation Hardness (MPa)H 358/30
Processing Methodinjection molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Hostacom AJ 1165 E BLACK Polypropylene, Fiber Grade
Mitsubishi Chemical Advanced Materials Plastic Composites GMTex® Glass-Mat-Reinforced Thermoplastic
Total PPH 12020 Polypropylene Homopolymer, Injection Molding
Braskem PH 3515 HOMO Polypropylene Homopolymer
Braskem HP 648S Injection Molding Polypropylene

PEQT8520 / 220155

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.