MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Polytek Poly 1512X Pourable Polyurethane Casting Resin
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Description: Poly 15-Series Liquid Plastics are excellent for casting decorative objects, production parts, tools, models, patterns, fixtures, duplicate masters, mold shells and more. Choose the 15-Series Liquid Plastic that’s best for your application: Poly 15-3 and 15-3X are dense, mineral-filled plastics with low shrinkage. For applications requiring water-clear, non-yellowing plastics, consider Poly-Optic® 14-Series products. For applications requiring spray application, consider EasyFlo-Series products.

Product Line Features:

  • Easy 1A:1B mix ratios
  • Reproduces fine detail
  • Can be machined, drilled and sanded
  • Tough and hard, but not brittle
  • Lightweight for mold shells
  • Low shrinkage upon cure
  • Fast-setting and slower-setting options
  • Low odor formula
  • Castable in large masses

Information provided by Polytek

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/cc
Viscosity 400 cPMixed
Linear Mold Shrinkage 0.0048 in/in
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 71
Tensile Strength 6712 psi
Elongation at Break 5.4 %
Modulus of Elasticity 118.3 ksi
Flexural Strength 10046 psi
@Strain 5.0 %
Flexural Modulus 241223 psi
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 142 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 0.500 - 4.00 hourDemold Time
Pot Life 5.00 min
 
Descriptive Properties
Cured ColorWhite
Maximum Exotherm251°F
Mix Ratio By Weight1A:1B
Specific Volume25.1 in3/lb

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPTK5087 / 251079

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.