MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Amodel® AS-4145 HS PPA, 45% glass fiber
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 50% Glass Fiber Reinforced

Material Notes: 45% glass fiber, for thick-wall parts (>3mm), fast cycle time, hot-water molds, heat stabilized, lubricated

Amodel® AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad temperature range, low moisture absorption, excellent chemical resistance and excellent electrical properties.

This resin is ideal for automotive electrical and electronic applications, including connectors, sockets, switches and sensors. It is also a good choice for under-hood enclosures that protect critical control systems such as anti-lock brakes, traction control, steering, electronic engine control, transmission and chassis control units. Its rapid crystallization rate and high flow can result in shorter cycles, thereby enhancing molding productivity and lowering costs.

- Black: AS-4145 HS BK 324

Applications: Abrasive Cleaning Material; Automotive Applications; Automotive Electronics; Automotive Under the Hood; Connectors; General Purpose; Housings; Industrial Applications; Industrial Parts; Lawn and Garden Equipment; Machine/Mechanical Parts; Metal Replacement; Thick-walled Parts; Valves/Valve Parts

Features: Chemical Resistant; Creep Resistant; Fast Molding Cycle; Good Dimensional Stability; Good Stiffness; Heat Stabilized; High Heat Resistance; High Strength; Hot Water Moldability; Low Moisture Absorption; Lubricated

Injection notes: Storage:
- Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® resins be dried prior to molding following the recommendations found in this datasheet and/or in the Amodel® processing guide.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.55 g/ccMethod A; ISO 1183
Water Absorption 0.21 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 cm/cmASTM D955
Linear Mold Shrinkage, Transverse 0.010 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 224 MPaISO 527-2
 228 MPaASTM D638
Elongation at Break 2.2 %ISO 527-2
 2.4 %ASTM D638
Tensile Modulus 15200 MPaASTM D638
 16100 MPaISO 527-2
Flexural Strength 327 MPaISO 178
Flexural Yield Strength 328 MPaASTM D790
Flexural Modulus 13100 MPaASTM D790
 13400 MPaISO 178
Compressive Strength 172 MPaASTM D695
Poissons Ratio 0.40ASTM E132
Shear Strength 89.6 MPaASTM D732
Izod Impact, Notched 100 J/mASTM D256
Izod Impact, Notched (ISO) 10.0 kJ/m²Type 1, Notch A; ISO 180
Charpy Impact Unnotched 63.0 kJ/m²Type 1, Edgewise; ISO 179
Charpy Impact, Notched 10.0 kJ/m²Type 1, Edgewise, Notch A; ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 8.00e+15 ohm-cmASTM D257
Dielectric Constant 3.7
@Frequency 1e+6 Hz
ASTM D150
 4.0
@Frequency 60 Hz
ASTM D150
Dielectric Strength 24.0 kV/mm
@Thickness 1.59 mm
ASTM D149
Dissipation Factor 0.0040
@Frequency 60 Hz
ASTM D150
 0.011
@Frequency 1e+6 Hz
ASTM D150
Comparative Tracking Index 600 VUL 746
High Voltage Arc-Tracking Rate, HVTR 13.0 mm/minUL 746
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 13.0 µm/m-°C
@Temperature 149 - 249 °C
ASTM E831
 16.0 µm/m-°C
@Temperature 0.000 - 90.0 °C
ASTM E831
CTE, linear, Transverse to Flow 59.0 µm/m-°C
@Temperature 0.000 - 90.0 °C
ASTM E831
 110 µm/m-°C
@Temperature 149 - 249 °C
ASTM E831
Melting Point 320 °CISO 11357-3
 320 °C
Maximum Service Temperature, Air 210 °CContinuous; ASTM D794
Deflection Temperature at 0.46 MPa (66 psi) >= 300 °C
@Thickness 3.18 mm
Annealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 298 °CUnannealed; ISO 75-2/A
 300 °C
@Thickness 3.18 mm
Annealed; ASTM D648
Flammability, UL94 HB
@Thickness 3.20 mm
 
Processing PropertiesOriginal ValueComments
Feed Temperature 79.0 °CInjection Hopper
Rear Barrel Temperature 318 - 324 °C
Front Barrel Temperature 327 - 332 °C
Melt Temperature 329 - 343 °CInjection
Mold Temperature 66.0 - 93.0 °C
Drying Temperature 121 °C
@Time 14400 sec
Moisture Content 0.030 - 0.060 %Injection
 
Descriptive Properties
AdditiveHeat Stabilizer; Lubricant; Mold Release
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorBlack
FormsPellets
ProcessingWater-Heated Mold Injection Molding
RoHS ComplianceYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4095 / 279895

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.