MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Precision Polymer Engineering Perlast® G75S Perfluoroelastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: Perlast® G75S has been specifically developed to cope with a wide range of process media, potent active pharmaceutical ingredients (APIs) and aggressive cleaning agents, being especially suited to withstand steam-in-place (SIP) and clean-in-place (CIP) procedures within pipe work and vessels. G75S is also suitable for other critical applications such as Water-For-Injection (WFI) systems. Perlast® G75S is an all round material that can be used for all types of applications requiring FDA and USP Class VI compliance. It is suitable for use in all product contact applications including dry, aqueous and fatty media. Unlike other FDA compliant elastomers, Perlast® G75S is thermally stable at higher temperatures, and is ideal for use in applications which require exposure to temperatures up to 310°C (590°F) making it suitable for use in Stage II Sterilization processes. Perlast® G75S is suitable for both dynamic and static applications and can be moulded into O-rings and custom shapes.

Applications: Recommended for use in pharmaceutical, bio-analytical and food processing applications, where both mechanical and chemical properties are crucial, and hygienic sealing capability is critical. Dynamic Seals: Split butterfly valve seals; Ball segment valve seals. Static Seals: O-rings; Pressure safety rings; Gaskets; Hygienic & sanitary couplings; Mechanical seals for stirring/mixing screws & pumps

Key Words: Rubbers
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 75ASTM D1415
 80ASTM D2240
Tensile Strength, Yield 19.0 MPaASTM D412
Elongation at Break 237 %ASTM D412
100% Modulus 0.00880 GPa
@Strain 100 %
ASTM D412
Compression Set 20 %
@Temperature 200 °C,
Time 259000 sec
ASTM D395
 
Thermal PropertiesOriginal ValueComments
CTE, linear 300 µm/m-°C
@Temperature 20.0 °C
Maximum Service Temperature, Air 310 °C
Minimum Service Temperature, Air -15.0 °C
 
Compliance PropertiesOriginal ValueComments
FDA Yes
USP Class VI Yes
 
Descriptive Properties
Colorwhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Greene Tweed CHEMRAZ® SD625 Perfluoroelastomer
Precision Polymer Engineering E70Q Ethylene Propylene Rubber
DuPont Mobility and Materials Kalrez® 8575 FFKM Perfluoroelastomer
Freudenberg Simriz® 483 Low Temperature FFKT Perfluoroelastomer Compound
Precision Polymer Engineering Perlast® G75B High Temperature Perfluoroelastomer

PPRECI025 / 57749

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.