MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Envalior Durethan® DP A 30 S FN30 DUS025 000000 Nylon 66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced, Flame Retardant

Material Notes: PA 66, non-reinforced, injection molding, halogen free flame retardant improved flowability

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.169 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.0010 cm/cmPost-shrinkage, 60x60x2; 120°C; 4 hour; ISO 294-4
 0.011 cm/cm60x60x2; 270°C / WZ 80°C; 600 bar; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0010 cm/cmPost-shrinkage, 60x60x2; 120°C; 4 hour; ISO 294-4
 0.011 cm/cm60x60x2; 270°C / WZ 80°C; 600 bar; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 50.0 MPacond.; ISO 527-1, -2; 50 mm/min
 85.0 MPad.a.m.; ISO 527-1, -2; 50 mm/min
Elongation at Yield 4.1 %d.a.m.; ISO 527-1, -2; 50 mm/min
 >= 20 %cond.; ISO 527-1, -2; 50 mm/min
Tensile Modulus 1500 MPacond.; ISO 527-1, -2; 1 mm/min
 3800 MPad.a.m.; ISO 527-1, -2; 1 mm/min
Flexural Strength 55.0 MPa
@Strain 8.0 %
cond., 2 mm/min; ISO 178-A
 135 MPa
@Strain 5.8 %
d.a.m., 2 mm/min; ISO 178-A
Flexural Yield Strength 40.0 MPa
@Strain 3.5 %
cond., 2 mm/min; ISO 178-A
 115 MPa
@Strain 3.5 %
d.a.m., 2 mm/min; ISO 178-A
Flexural Modulus 1600 MPacond., 2 mm/min; ISO 178-A
 3900 MPad.a.m., 2 mm/min; ISO 178-A
Izod Impact, Notched (ISO) <= 10.0 kJ/m²d.a.m.; ISO 180-1A
 <= 10.0 kJ/m²cond.; ISO 180-1A
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
@Temperature 23.0 °C
d.a.m.; ISO 180-1U
 45.0 kJ/m²
@Temperature -30.0 °C
d.a.m.; ISO 180-1U
 55.0 kJ/m²
@Temperature -30.0 °C
cond.; ISO 180-1U
 NB
@Temperature 23.0 °C
cond.; ISO 180-1U
Charpy Impact Unnotched 50.0 kJ/m²
@Temperature -30.0 °C
d.a.m.; ISO 179-1eU
 60.0 kJ/m²
@Temperature 23.0 °C
d.a.m.; ISO 179-1eU
 80.0 kJ/m²
@Temperature -30.0 °C
cond.; ISO 179-1eU
 NB
@Temperature 23.0 °C
cond.; ISO 179-1eU
Charpy Impact, Notched <= 10.0 kJ/m²d.a.m.; ISO 179-1eA
 <= 10.0 kJ/m²cond.; ISO 179-1eA
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 600 Vd.a.m.; Solution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 80.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1, -2
CTE, linear, Transverse to Flow 70.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1, -2
Melting Point 265 °C10°C/min; ISO 11357-1, -3
Deflection Temperature at 0.46 MPa (66 psi) 212 °CISO 75-1, -2
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °CISO 75-1, -2
Vicat Softening Point 230 °C
@Load 5.10 kg
120°C/hour; ISO 306
Flammability, UL94 V-0
@Thickness 0.400 mm
Oxygen Index 35 %Method A; ISO 4589-2
Glow Wire Ignition Temperature 775 °C
@Diameter 0.400 mm
IEC 60695-2-13
Glow Wire Flammability Index 960 °C
@Diameter 0.400 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Melt Temperature 260 °Cfor test specimens; ISO 294
 260 - 270 °C
Mold Temperature 80.0 °Cfor test specimens; ISO 294
 80.0 - 100 °C
Drying Temperature 80.0 °C
Dry Time 2 - 6 hour
Moisture Content 0.030 - 0.070 %residual; Karl Fischer Test
 
Descriptive Properties
ISO Short NameISO 1874-PA 66, GF, 14-040; ISO 1043 PA FR(30)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® B3UGM210 GR 22866 10/50% Glass/Mineral Filled PA6 FR (Dry)
BASF Ultramid® B3UGM210 GR 22866 10/50% Glass/Mineral Filled PA6 FR (Conditioned)
Oceanchem Group Melamine Polyphosphate (MPP)
Overview of materials for Nylon 6 Fiber
Lanxess Durethan® DP A 30 S FN30 000000 Nylon 66

PLANX0644 / 133607

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.