Lupolen 3026 K is an additivated, low density polyethylene. It contains slip and anti-blocking agent. It is characterized by a good processability. LyondellBasell customers report that films made from Lupolen 3026 K exhibit a glossy surface finish. Lupolen 3026 K provides the option to produce films with very good optical properties. It is delivered in pellet form. This product is not intended for use in medical and pharmaceutical applications. Applications: Food Packaging Film, Lamination Film, Shrink FilmInformation provided by LyondellBasell. |