MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Eastman Eastar™ Renew AN014-30 Natural Copolyester
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Eastar™ Renew copolyester AN014-30 Natural is a high flow product that contains mold release. Other features include excellent appearance and clarity, good physical properties, chemical resistance, and ease of melt processing with an increase of 20-40% in flow length over copolyester AN004-30 Natural, as determined by spiral flow testing. This high flow product is especially suited for those applications utilizing thin-walled intricate tools. Eastar™ Renew copolyester AN014-30 Natural is approved for food contact and thereby under existing United States Food and Drug Administration (FDA) regulations, it may be used in food contact articles which comply with the specifications and conditions of use in 21 CFR 177.1240. Eastman Renew polymers have been certified by International Sustainability & Carbon Certification (ISCC), a global, independent agency for tracking sustainable content in a variety of industries. Renew polymers are produced with ISCC certified circular content by mass balance allocation. This product has been GREENGUARD INDOOR AIR QUALITY CERTIFIED. The GREENGUARD INDOOR AIR QUALITY CERTIFIED Mark is a registered certification mark used under license through the GREENGUARD Environmental Institute (GEI). GEI is an industry-independent, non-profit organization that oversees the GREENGUARD Certification Program. The GREENGUARD Certification Program is an industry independent, third-party testing program for low-emitting products and materials for indoor environments. For more information about GEI and to obtain printable certificates for Eastman™ Copolyesters, visit www.greenguard.org. Choose Eastman Chemical Company under the Manufacturer category and click search to display a list of our products.

Applications

  • Bottles-fragrance pkg
  • Closures-fragrance pkg
  • Color cosmetics packaging
  • Fragrance packaging
  • Jars-skin care pkg
  • Personal care & cosmetics packaging
  • Personal care packaging
  • Skin care packaging

Information provided by Eastman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccASTM D792
Water Absorption 0.150 %
@Time 86400 sec
immersion; ASTM D570
Linear Mold Shrinkage 0.00300 in/inASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 107ASTM D785
Tensile Strength at Break 43.0 MPaASTM D638
Tensile Strength, Yield 50.0 MPaASTM D638
Elongation at Break 270 %ASTM D638
Elongation at Yield 5.00 %ASTM D638
Flexural Yield Strength 68.0 MPaASTM D790
Flexural Modulus 1900 MPaASTM D790
Izod Impact, Notched 44.0 J/m
@Temperature -40.0 °C
ASTM D256
 80.0 J/m
@Temperature 23.0 °C
ASTM D256
Izod Impact, Unnotched NB
@Temperature 23.0 °C
ASTM D4812
 NB
@Temperature -40.0 °C
ASTM D4812
Puncture Energy 38.0 J
@Temperature -40.0 °C
@ Max. Load; ASTM D3763
 40.0 J
@Temperature 23.0 °C
@ Max. Load; ASTM D3763
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 73.0 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 66.0 °CASTM D648
Vicat Softening Point 86.0 °C
@Load 1.00 kg
ASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze <= 1.00 %ASTM D1003
Transmission, Visible 92.0 %Total; ASTM D1003
 
Processing PropertiesOriginal ValueComments
Melt Temperature 230 - 280 °C
Mold Temperature 15.0 - 30.0 °C
Drying Temperature 70.0 °C
Dry Time 4.00 hour
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM4119 / 323742

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.