MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Plenco PlasGlas™ 40118 High Strength Glass Filled Thermoset Polyester BMC  (discontinued **)
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Polyester, TS; Thermoset Polyester Glass Filled BMC

Material Notes: PlasGlas 40118 is a specially formulated glass-filled polyester bulk molding compound intended for use as a floor tile material. As such, it has superior flammability ratings, low smoke generation, and excellent smoke toxicity ratings. It is offered in bulk or extruded form, and is currently available in natural. Other colors available upon request.

Data provided by Plaslok Corporation.

Plaslok Corporation was purchased by Plastics Engineering Company in March 2000. The Plaslok name is no longer used on any products.

Key Words: Bulk Molding Compound
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.90 g/ccASTM D792
Water Absorption 0.15 %ASTM D570
Linear Mold Shrinkage 0.0020 cm/cmCompression; ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Barcol 60ASTM D2583
Tensile Strength, Ultimate 35.0 MPaASTM D638
Flexural Yield Strength 75.0 MPaASTM D790
Flexural Modulus 13.0 GPaASTM D790
Compressive Yield Strength 124 MPaASTM D695
Izod Impact, Notched 4.27 J/cmASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 260 °CASTM D648
Flammability, UL94 V-0
@Thickness 0.740 mm
 V-0
@Thickness 0.740 mm
Oxygen Index 66 %ASTM D2863

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Polynt 30 CF60- 6mm Carbon Fiber VE BMC
Polynt BMC 580 Bulk Molding Compound Green Compound With Natural Fiber
A. Schulman Premi-Glas® 1100-20 Fiberglass Reinforced Thermoset BMC
Plenco PlasGlas™ 20415 Low Shrinkage Electrical Thermoset Polyester BMC
Plenco PlasGlas™ 50112 Heat Resistant Glass Filled Thermoset Polyester BMC

PLEO931 / 50819

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.