LNP STAT-KON DX07323 compound is based on Polycarbonate (PC) resin containing stainless steel fiber. Added features of this grade include: Electrically Conductive, Impact Modified, meet ATEX requirements. Features: Impact Modified,Electrically Conductive Information provided by SABIC |