Description: Liquid two-part epoxy adhesive filled with microspheres. Its low viscosity allows to be used for filling, potting and fastening inserts applications. Features: - Room temperature cure (= 18°C/ 64°F)
- Low density: Filled with ˜ 12 % of glass microspheres with a density of 0,2 (crush-resistance: 1000 PSI / 6,9 MPa)
- Outstanding mechanical properties over a wide range of temperature
Information provided by Hexcel Corporation. |