MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese FORTRON 6850L6 PPS, 50% Mineral / Glass Reinforced
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled

Material Notes: Fortron 6850L6 offers the lowest warpage available. The easy flowing nature allows this product to be injection molded into thin walled applications. The excellent balance of mineral and glass fibers result in a superior heat resistance and dimensional stability. This grade is inherently flame-retardant along with high hardness and rigidity. Especially used for thin walled by unfavorable flow length-wall thickness ratio. This is the most isotropic grade available.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.80 g/ccASTM D792
Density 1.80 g/ccISO 1183
Water Absorption 0.020 %
@Temperature 22.8 °C
24hr immersion; ASTM D570
Water Absorption at Saturation 0.020 %ISO 62
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cmASTM D955
 0.0030 - 0.0060 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.0030 - 0.0050 cm/cmASTM D955
 0.0040 - 0.0060 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 96ISO 2039-2
 96ASTM D785
Tensile Strength at Break 125 MPa5mm/min; ISO 527-2/1A
 18000 psiASTM D638
Elongation at Break 1.0 %5mm/min; ISO 527-2/1A
 1.0 %ASTM D638
Tensile Modulus 18500 MPa50mm/min; ISO 527-2/1A
Flexural Strength 190 MPaISO 178
 28000 psiASTM D790
Flexural Modulus 16800 MPaISO 178
 2.40e+6 psiASTM D790
Izod Impact, Notched 0.800 ft-lb/inASTM D256
Izod Impact, Unnotched 5.00 ft-lb/inASTM D256
Izod Impact, Notched (ISO) 4.00 kJ/m²
@Temperature -30.0 °C
ISO 180/1A
 20.0 kJ/m²
@Temperature 23.0 °C
ISO 180/1U
Charpy Impact Unnotched 16.0 kJ/m²ISO 179/1eU
 16.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 4.00 kJ/m²ISO 179/1eA
 4.00 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
 1.00e+17 ohm-cmASTM D257
Surface Resistance >= 1.00e+15 ohmIEC 60093
Dielectric Strength 25.0 kV/mmIEC 60243-1
Dissipation Factor 0.0010
@Frequency 1e+6 Hz
IEC 60250
Arc Resistance 182 secASTM D495
Comparative Tracking Index 225 VASTM D3638
 225 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 15.0 µm/m-°CISO 11359-2
CTE, linear, Transverse to Flow 31.0 µm/m-°CISO 11359-2
Melting Point 280 °C10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 0.46 MPa (66 psi) 536 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 270 °CISO 75-1, -2
 500 °FASTM D648
Deflection Temperature at 8.0 MPa 215 °CISO 75-1, -2
Glass Transition Temp, Tg 90.0 °CISO 11357-1,-2,-3
Flammability, UL94 V-0
@Thickness 1.50 mm
 V-0
@Thickness 0.380 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 140 - 160 °Ccavity
 330 - 340 °Chot runner
Feed Temperature 60.0 - 80.0 °C
Zone 1 290 - 300 °C
Zone 2 310 - 320 °C
Zone 3 330 - 340 °C
Zone 4 330 - 340 °C
Die Temperature 310 - 330 °C
Melt Temperature 310 - 340 °CISO 294
 330 - 340 °C
Mold Temperature 135 - 160 °CISO 294
Drying Temperature 130 - 140 °C
Dry Time 3.00 - 4.00 hour
Moisture Content <= 0.020 %
Injection Pressure 50.0 - 100 MPa
Hold Pressure 30.0 - 70.0 MPa
Back Pressure <= 3.00 MPa
Screw Speed 50 rpm
@Diameter 55.0 mm
 75 rpm
@Diameter 40.0 mm
 120 rpm
@Diameter 25.0 mm
 
Descriptive Properties
Injection moldingYes
Injection speedfast
Sheet extrusionNo

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese FORTRON 4184L4 PPS, 53% Mineral / Glass Reinforced
Celanese FORTRON 11400000000 PPS, 40% Glass Reinforced
Celanese FORTRON 4184L6 PPS, 53% Mineral / Glass Reinforced
Celanese FORTRON ICE 714A PPS, 65% Mineral / Glass Reinforced
Celanese FORTRON 1140L0 PPS, 40% Glass Reinforced

PHCQ289 / 178744

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.