MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Dow Nordel® NDR 46140.01 EPDM Hydrocarbon Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Description: NDR 46140.01 is a developmental product in granular form that contains carbon black as a partitioning agent. It is a very high molecular weight, amorphous EPDM grade with a fast cure rate. It also offers an excellent combination of:
  • very fast mixing with good dispersion level
  • excellent tensile strength and compression set resistance, even at very high loading
It was designed for highly extended compounds to be used in applications such as extruded profiles, hose and seals.

Information provided by manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.970 g/ccASTM D297
Volatiles <= 0.40 %Total Volatiles; DuPont Dow EPRG-21
Mooney Viscosity 140
@Temperature 125 °C
Polymer (calculated), ML 1 + 4
 
Descriptive Properties
Carbon Black Content (N650)30 phrDuPont Dow EPRG-2
ENB4.9 mass%ASTM D6047
Ethylene58 mass%ASTM D3900

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Nordel® NDR 4820P EPDM Hydrocarbon Rubber
Dow Nordel® IP 4770P EPDM Hydrocarbon Rubber
Dow Nordel® NDR 3722P EPDM Hydrocarbon Rubber
Dow Nordel® IP 4725P High Hardness Extruded Profile
Dow Nordel® IP 4760P Compound

PDVG48 / 34168

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.