MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Sibur ABS-C Molding Grade ABS Plastic
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: With high resistance to burning for bodies of devices, technical articles and consumer goods, and contacting with good products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Absorption <= 0.30 %
Melt Index of Compound 7.0 g/10 min
 
Chemical PropertiesOriginal ValueComments
Styrene Content <= 0.050 %
 
Mechanical PropertiesOriginal ValueComments
Elongation at Break >= 8.0 %
Izod Impact, Notched (ISO) >= 5.00 kJ/m²
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point <= 95.0 °C
 
Descriptive Properties
Acrylonitrile Content<.001
Impact Tension Strength>5 MPa
Resistance to BurningPB-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
OJSC Plastic ABS 2020-31 ABS Plastic
Lucite International Perspex™ XT IM50 Acrylic Extruded Sheet
Lucite International Perspex™ GS Acrylic Cast Sheet 000/0000
Sibur ABS 1530 Molding Grade ABS Plastic
Sibur ABS 2020-30M Molding Grade ABS Plastic

PSIB038 / 67601

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.