MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Danquinsa DANCURE® 246-13 Isocyanate Hardeners
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: DANCURE® 246-13 is a high solid isocyanate hardener for universal use in paints, coating compounds for textile- and building industry, for adhesives and primers.

Application: In the processing of solvent-based coatings and adhesive systems, DANCURE® 246-13 serves as a hardener. Also as a curing agent for PUR-cover coatings and PUR-lamination coatings in the process of textile coating, DANCURE® 246-13 has proved as a product with best results. For many years, the curing of reactive acrylatehas been carried out with this product. In conjunction with poly hydroxyl products and coal tar, DANCURE® 246-13 is also suitable for the production of air dried one- respective two component polyurethane coatings.

Information provided by Danquinsa GMBH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.17 g/ccDIN 51.757
Solids Content 73 - 77 %DIN 53.189
Brookfield Viscosity 1000 - 3000 cPRVT
 
Thermal PropertiesOriginal ValueComments
Flash Point 1.00 °CDIN 51.755
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 4.01933
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
 
Descriptive Properties
Aspectclear and lightly yellowish liquid
Composition<0.5%Free TDI content
 8-18%NCO
SolventEthylene acetate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDANQ109 / 294529

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.