MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
CMW® ELKONIUM 72 gold based alloy  (discontinued **)
Categories: Metal; Nonferrous Metal; Precious Metal; Gold Alloy

Material Notes: This material has been rebranded as a part of the NAECO® ELKONIUM® product line.

Pure gold has complete resistance to atmospheric tarnish and oxidation. It does not contribute to polymer formations like platinum and palladium alloys. Wrought gold metal is very soft and prone to welding and has very few contact applications. Electroplated coatings of gold on silver and other base metals are used in dry circuit application and to provide long shelf life reliability. Gold is alloyed with other metals to improve hardness, contact performance, and reduce cost.

ELKONIUM® 72 is the trademark used by CMW for a gold-silver-platinum alloy that is harder and more resistant to mechanical wear than ELKONIUM 70 alloy. It is completely resistant to atmospheric corrosion at normal temperatures, and is widely used in telephone relays and other sensitive switching devices. It offers good wear resistant and a low contact resistance when used as a brush contact and operated against other noble metal surfaces in sliding contact applications.

Information provided by CMW Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 16.0 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell 15T 70annealed
 84cold worked
Tensile Strength, Ultimate 40000 psiannealed
 60000 psicold worked
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000156 ohm-cm11 % IACS
 
Component Elements PropertiesOriginal ValueComments
Gold, Au 69 %
Platinum, Pt 6.0 %
Silver, Ag 25 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NCMW112 / 15929

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.