MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
ChevronTexaco Saturating Wax 2
Categories: Fluid; Lubricant

Material Notes: Features

Chevron Saturating Wax 2 is a food grade blend of fully refined paraffin wax and a wet strength additive. It is specifically formulated to impart moisture resistance and structural strength to corrugated paperboard and boxes and is ideally suited for wax saturating and wax cascading operations.

Chevron Saturating Wax 2 has properties typical of high purity paraffin wax. When heated above its melting point, it becomes a colorless, low viscosity liquid with low odor. When cooled below its melting point, it hardens to become opaque, semicrystalline solid.

Significant advantages of Chevron Saturating Wax 2 are its high melting point, high blocking point and high degree of hardness. Consequently, it dries quickly allowing for higher cascader rates, is less likely to allow boxes to fuse or laminate when stacked, especially in warmer climates and provides greater protection against scuffing.

Chevron Saturating Wax 2 contains food grade BHT to prevent oxidation that can cause degradation and discoloration.

Chevron Saturating Wax 2 complies with U.S. Food and Drug Administration (FDA) regulations pertaining to the use of petroleum wax as a component paper and paperboard in contact with aqueous and fatty foods (21 CFR 176.170) and dry foods (21 CFR 176.180).

Chevron Saturating Wax 2 is also approved by the U.S. Department of Agriculture (USDA) for use in packaging for meat, fish, rabbit, and poultry packed under federal inspection.

Applications

Chevron Saturating Wax 2 is ideally suited for saturating corrugated boxes used to ship and store fresh produce, meat, poultry, and fish.

Treating corrugated boxes with Chevron Saturating Wax 2, at levels between 35% and 50%, enhances the dry strength of the boxes and protects against loss of strength caused by contact with liquid water and water vapor.

Chevron Saturating Wax 2 may be applied to corrugated paperboard by means of dipping or cascading. Applications temperatures typically range between 190°F and 205°F. The optimal application temperature will depend on the application method, the size and weight of the paperboard, and the desired appearance of the waxed surface.

Key Words: CPS Number: 260312; MSDS Number: 1187
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.7716 g/cc
@Temperature 82.2 °C
ASTM D4052
Kinematic Viscosity at 100°C (212°F) 5.6 cStASTM D445
 
Mechanical PropertiesOriginal ValueComments
Penetration 10
@Thickness 0.100 mm,
Temperature 25.0 °C
 18 - 55
@Thickness 0.100 mm,
Temperature 37.8 °C
 
Thermal PropertiesOriginal ValueComments
Melting Point 137 °F
Flash Point 450 °CASTM D92
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
Blocking Point, °F115
Cloud Point, °F165
Color+28, Saybolt
Oil Content wt%0.3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ChevronTexaco 141 Refined Wax
Michelman® Michem® Emulsion 80939M Nonionic paraffin wax emulsion
Michelman® Michem® Lube 180 Anionic co-emulsion of carnauba and paraffin waxes
BASF Octadecyl Vinyl Ether
Evonik VESTOWAX® SH 105 Powder Paraffin Wax

WCHEV387 / 75002

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.