MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Arkema KYNAR FLEX® 2750-01 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF); Polyvinylidinefluoride (PVDF), Molded/Extruded

Material Notes: Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistance; high purity

Applications:

  • Chemical processing – production, storage and transfer of corrosive fluids
  • Electronics – protective sheathing, plenum and wiring insulation
  • Semi-conductor industry
  • Food stuff and Healthcare industries
  • Transportation – fuel line and pipe, thermoformed body components

Information provided by Arkema Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.78 - 1.80 g/ccASTM D792
Density 1.78 g/ccISO 1183
Water Absorption 0.030 %Dry; Sim. to ISO 62
 0.030 - 0.060 %ASTM D570
Viscosity 2.00e+6 - 2.50e+6 cP
@Shear Rate 100 1/s,
Temperature 230 °C
Melt; ASTM D3835
Melt Flow 1.9 g/10 min
@Load 5.00 kg,
Temperature 230 °C
cm³/10 min Volumetric Rate; ISO 1133
 4.0 - 14 g/10 min
@Load 12.5 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 57 - 62ASTM D2240
Tensile Strength at Break 20.0 - 27.6 MPaASTM D638
Tensile Strength, Yield 13.8 - 21.4 MPaASTM D638
 21.0 MPaDry; ISO 527-1/-2
Elongation at Break >= 50 %Dry; ISO 527-1/-2
 200 - 400 %ASTM D638
Elongation at Yield 15 %Dry; ISO 527-1/-2
 15 - 25 %ASTM D638
Tensile Modulus 276 - 448 MPaASTM D638
 526 MPaDry; ISO 527-1/-2
Flexural Strength 13.8 - 24.1 MPa
@Strain 5.0 %
ASTM D790
Flexural Modulus 276 - 414 MPaASTM D790
Compressive Strength 24.1 - 31.0 MPaASTM D695
Izod Impact, Notched NBASTM D256
Charpy Impact, Notched NB
@Temperature 23.0 °C
Dry; ISO 179/1eA
Coefficient of Friction, Dynamic 0.54vs. steel; ASTM D1894
Coefficient of Friction, Static 0.55vs. steel; ASTM D1894
Taber Abrasion, mg/1000 Cycles 21 - 25CS 17 1000g:pad; ASTM-G195-13A
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.00e+14 ohm-cm65% R.H; ASTM D257
 2.00e+14 ohm-cmDry; IEC 60093
Surface Resistivity per Square 4.80e+11 - 5.10e+11 ohmASTM D257
Dielectric Constant 7.0
@Frequency 1e+6 Hz
Dry; IEC 60250
 3.8 - 12.1
@Frequency 1000 Hz
ASTM D150
 11.5
@Frequency 100 Hz
Dry; IEC 60250
Dielectric Strength 1.10 - 1.30 kV/mmASTM D149
Dissipation Factor 0.024
@Frequency 100 Hz
Dry; IEC 60250
 0.020 - 0.24
@Frequency 100000 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 162 - 216 µm/m-°CASTM D696
CTE, linear, Parallel to Flow 177 µm/m-°CDry; ISO 11359-1/-2
Specific Heat Capacity 0.745 - 0.958 J/g-°CDSC
Thermal Conductivity 0.144 - 0.180 W/m-KASTM D433
Melting Point 130 - 138 °CASTM D3418
 134 °C10°C/min; Dry; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 57.0 °CDry; ISO 75-1/-2
 48.9 - 65.6 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 43.0 °CDry; ISO 75-1/-2
 35.0 - 51.7 °CASTM D648
Vicat Softening Point 61.0 °C50°C/h 50N; Dry; ISO 306
Glass Transition Temp, Tg -40.0 °CASTM D7028
 -40.0 °C10°C/min; Dry; ISO 11357-1/-2
Decomposition Temperature 375 °C1% wt. loss, TGA, in air
 410 °C1% wt. loss, TGA, in nitrogen
Flammability, UL94 V-0
@Thickness 0.800 mm
IEC 60695-11-10
 V-0
@Thickness 1.60 mm
IEC 60695-11-10
Oxygen Index 43 %ASTM D2863
 49 %Dry; ISO 4589-1/-2
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.41sodium D line; ASTM D542
 
Processing PropertiesOriginal ValueComments
Melt Temperature 240 °CInjection Molding; ISO 294
Mold Temperature 60.0 °CInjection Molding; ISO 10724
Injection Velocity 10.0 mm/secInjection Molding; ISO 294
Hold Pressure 13.0 MPaInjection Molding; ISO 294
 
Descriptive Properties
Form as DeliveredPellets
Heat StabilizedYes
Light StabilizedYes
Moisture SensitiveNo
Processing MethodsInjection Molding
 Other Extrusion
 Sheet Extrusion
 Transfer Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema KYNAR FLEX® 2800-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Arkema KYNAR FLEX® 2850-00 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Arkema KYNAR FLEX® 2800-00 Polyvinylidene Fluoride Copolymer - Extrusion
Arkema KYNAR FLEX® 2950-05 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Arkema KYNAR FLEX® 2850-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding

PARKG914 / 144539

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.